Test nº 1.
3 minutes silver bath  (Ph 4.5)
10 sec. Exposition at f 4.5 (Calumet Caltar II 210)
Liquids 18º
Cloudy day, 17.00h
Collodion 1 week old
Developer brand new.
(The big mess..)


Test nº 2.
3 minutes silver bath  (Ph 4.5)
30 sec. Exposition at f 4.5 (Calumet Caltar II 210)
Liquids 18º
Cloudy day, 17.00h
Collodion 1 week old
Developer brand new.
(Good contrast...)


Test nº 3.
3 minutes silver bath  (Ph 4.5)
60 sec. Exposition at f 4.5 (Calumet CaltarII 210)
Liquids 18º
Cloudy day, 17.00h
Collodion 1 week old
Developer brand new.
(Big problems with peeling..!!)